Low-Hydrogen Iron Powder Welding Electrode for Carbon and Low-Alloy Steel

Low-Hydrogen Iron Powder Welding Electrode for Carbon and Low-Alloy Steel

Brand NameHangzhou MetalWire Technology
Model NumberE7018
MOQ1 set
PriceNegotiable
Delivery Time45-60 days
Payment TermsT/T, L/C

Product Description

1. Overview

The low-hydrogen iron powder welding electrode features a basic coating and is designed for all-position welding of carbon steel and low-alloy steel structures. The iron powder coating promotes a stable arc and high deposition efficiency.

1.1 Standards

Standard Classification
AWS A5.1 E7018
GB/T 5117 E5018
ISO 2560-B E 49 18 A

2. Coating and Operating Characteristics

  • Coating: iron powder with low-hydrogen potassium; suitable for AC and DC welding.
  • Stable arc, low spatter, and easy slag removal.
  • High deposition efficiency and good weld appearance.
  • All-position welding: flat, horizontal, vertical, and overhead.
  • Typical applications: carbon steel and low-alloy steel structures, such as 16Mn.

3. Deposited Metal Chemical Composition (%)

Element C Mn Si S P Ni Cr Mo V
Guaranteed ≤ 0.15 ≤ 1.60 ≤ 0.90 ≤ 0.035 ≤ 0.035 ≤ 0.30 ≤ 0.20 ≤ 0.30 ≤ 0.08
Typical 0.077 1.07 0.54 0.005 0.014 0.011 0.028 0.007 0.016

4. Deposited Metal Mechanical Properties

Property Tensile strength (Rm) Yield strength (ReL) Elongation (A) Impact energy (KV2) at -30 °C
Guaranteed ≥ 490 MPa ≥ 400 MPa ≥ 20% ≥ 27 J
Typical 550 MPa 455 MPa 32% 156 J

X-ray inspection: Grade I (defect-free).

5. Recommended Welding Current

Diameter (mm) 2.5 3.2 4.0 5.0
Current (A), AC/DC 60–100 80–140 110–210 160–230

6. Welding Positions and Operating Notes

The electrode is suitable for all-position welding: flat, horizontal, vertical, and overhead.

  1. Dry the electrodes at 350 °C for 1 hour before use.
  2. Remove rust, oil, moisture, and other contaminants from the workpiece.
  3. Keep the arc short and avoid excessive arc elongation.
  4. Clean slag between passes in multi-layer welding.
View More