Continuous Hot-Dip Galvanizing Line for Steel Sheet
| Brand Name | Hangzhou MetalWire Technology |
|---|---|
| Model Number | RST-RDX-003 |
| MOQ | 1 set |
| Price | Negotiable |
| Delivery Time | 45-60 days |
| Payment Terms | T/T, L/C |
Product Description
1. Overview
The continuous hot-dip galvanizing line for steel sheet processes cold-rolled carbon steel and low-alloy steel coils into zinc-coated strip. Cleaning, annealing, zinc immersion, coating-weight control, cooling, skin pass, tension leveling, passivation, and oiling are carried out in one continuous operation.
The line is suitable for construction, appliance manufacturing, automotive, and general fabrication markets that require a consistent coating, controlled spangle, and good formability.
2. Raw Material and Product Range
| Item | Specification |
|---|---|
| Base material | Cold-rolled carbon structural steel, high-quality cold-rolled carbon structural steel, and low-alloy steel |
| Strip width | 600–1500 mm |
| Strip thickness | 0.15–3.5 mm |
| Coil outer diameter | Ø800–2000 mm |
| Process speed | 80–200 m/min |
| Energy | Electricity, gas, liquefied petroleum gas, steam, and compressed air |
| Coating appearance | Regular spangle, small spangle, no spangle, or finishing spangle |
| Coating weight | 50–300 g/m² (both sides) |
| Post-coating treatment | Skin pass, tension leveling, fingerprint-resistant coating or passivation, and oiling |
3. Process Flow
Coil loading → uncoiling → strip welding → cleaning → annealing → zinc immersion → air-knife coating control → cooling → skin pass → tension leveling → passivation → oiling → recoiling
4. Key Systems
4.1 Entry and Exit Section
The entry section handles coil loading, uncoiling, shearing, and welding. The exit section performs tension control, recoiling, and coil discharge.
4.2 Cleaning and Annealing
The strip is cleaned before entering the annealing furnace. Controlled heating and cooling prepare the steel surface for a uniform zinc-iron reaction and help develop the required mechanical properties.
4.3 Zinc Kettle and Air Knife
The strip passes through the molten-zinc bath and then through an air knife. The air-knife pressure and position control the coating weight on each side of the strip.
4.4 Skin Pass and Tension Leveling
Skin pass improves surface quality and strip shape. Tension leveling corrects strip flatness and reduces residual stress before passivation and oiling.
4.5 Surface Treatment
Passivation or fingerprint-resistant coating protects the zinc surface during storage and transport. Oiling further improves corrosion protection and handling.
5. Quality Control
- Strip thickness, width, and flatness are monitored throughout the line.
- Coating weight is controlled by the air knife and checked across the strip width.
- Spangle and surface appearance are selected according to the end application.
- Skin pass and tension leveling parameters are adjusted for the required surface finish and mechanical properties.
6. Applications
- Roofing, wall panels, and building envelopes
- Home appliances and HVAC equipment
- Automotive structural and body panels
- Furniture, shelving, and general sheet-metal products